Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.43 - 5.75 GPa | 788 - 834 ksi | Calculated |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |