Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.10 - 5.19 GPa | 450 - 753 ksi | Average value: 4.40 GPa Grade Count:3 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |