Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.477 - 3.05 GPa | 69.2 - 443 ksi | Average value: 1.44 GPa Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |