Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.58 GPa | 809 ksi | Calculated |
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Shear Modulus | 5.58 GPa | 809 ksi | Calculated |
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |