Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 5.46 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 5.46 - 5.98 GPa
792 - 867 ksi
Average value: 5.76 GPa Grade Count:3
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Shear Modulus 5.46 GPa
792 ksi
Calculated
Plenco 6401 Phenolic, Granular, Compression Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Shear Modulus 5.46 GPa
792 ksi
Calculated
Plenco 6500 Phenolic, Briquette, Transfer Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..
Copyright © lookpolymers.com All Rights Reserved