Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.10 GPa | 740 ksi | Calculated |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Shear Modulus | 5.10 GPa | 740 ksi | in <110> direction |
Mateck Potassium Bromide (KBr) Optical crystals |
|||
Shear Modulus | 5.10 GPa @Temperature 23.0 °C |
740 ksi @Temperature 73.4 °F |
In-Plane; prEN6032 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS Fiber: AS7 GS, UD, 150 g/m2Information provided by HexCel |