Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 44.1 GPa | 6400 ksi | |
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |