Polymer Property : Shear Modulus = 4.92 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 4.92 GPa
714 ksi
Calculated
Plenco 1581 Polyester, Briquette, Transfer Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..