Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Piezo Kinetics 700 Lead Zirconate Titanate Piezoelectric This material has low dielectric constant, high QM, high shear coupling coefficient, good temperature stability and low aging characteristics. Common use of this material is in delay lines and accel.. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-BASF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-BK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-PSK3 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-SK14 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-SSK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-SSK8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott P-SF8 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 34.0 GPa | 4930 ksi | calculated |
Schott N-LAK12 Glass Information Provided by SCHOTT North America, Inc. |