Calculated
CoorsTek AD-94 Alumina (nom. 94% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Shear Modulus 125 GPa
18100 ksi
Calculated
CoorsTek AD-96 Alumina (nom. 96% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Shear Modulus 125 GPa
18100 ksi
Calculated
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
Shear Modulus 125 GPa
18100 ksi
Calculated
CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Shear Modulus 125 GPa
18100 ksi
calculated
Ceradyne Ceralloy® 147-5 Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's..