Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 124 GPa | 18000 ksi | Calculated |
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4) EKatherm® Silicon Nitride is the state-of-the-art material for a wide variety of components used in Aluminum Alloy casting processes.Features: High Temperature Resistance High Thermal Shock Resist.. |