Mechanical Properties Metric English Comments
Shear Modulus 1.32 - 1.44 GPa
191 - 209 ksi
Calculated
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Shear Modulus 1.32 - 4.10 GPa
191 - 595 ksi
Average value: 2.61 GPa Grade Count:8
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..