Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.200 GPa | 29.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.200 GPa | 29.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-327 - 3/8 - 4.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Modulus | 0.200 GPa | 29.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Modulus | 0.200 GPa | 29.0 ksi | torsional |
DSM Fibre Intermediates Nyrim® 4000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Shear Modulus | 0.200 GPa | 29.0 ksi | |
Cymat A35620SC 020SS Stabilized Aluminum Foam Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it .. |
|||
Shear Modulus | 0.200 - 1.00 GPa @Temperature 50.0 - 225 °C |
29.0 - 145 ksi @Temperature 122 - 437 °F |
Average value: 0.762 GPa Grade Count:7 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Shear Modulus | 0.200 - 1.00 GPa @Temperature 50.0 - 225 °C |
29.0 - 145 ksi @Temperature 122 - 437 °F |
Average value: 0.762 GPa Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Shear Modulus | 0.200 - 1.00 GPa @Temperature 50.0 - 225 °C |
29.0 - 145 ksi @Temperature 122 - 437 °F |
Average value: 0.762 GPa Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |