Polymer Property : Shear Modulus = 0.178 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.178 GPa
25.8 ksi
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..