Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/4-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 3/8-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/8-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-327 - 3/16 - 6.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, L Direction, preliminary value obtained from limited testing |
Hexcel® HexWeb® HRH-78 - 1/8 - 8.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP/F35 - 3.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP/OX - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Modulus | 0.103 GPa | 15.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Modulus | 0.103 GPa | 14.9 ksi | ASTM C273 |
3A Composites Core Materials AIREX® PXw.420 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |