Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0986 GPa | 14.3 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |