Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0724 GPa | 10.5 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/4-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.0724 GPa | 10.5 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10/F50 - 5.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglass cloth reinforc.. |
|||
Shear Modulus | 0.0724 GPa | 10.5 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.0724 GPa | 10.5 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |