Polymer Property : Shear Modulus = 0.0483 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0483 GPa
7.00 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Modulus 0.0483 GPa
7.00 ksi
Plate Shear, W Direction
Hexcel® HexWeb® HRH-36 - 5/32 - 2.4 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Modulus 0.0483 GPa
7.00 ksi
Plate Shear, W Direction, typical value
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.0 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..
Shear Modulus 0.0483 GPa
7.00 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP/OX - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Modulus 0.0483 GPa
7.00 ksi
Plate Shear, W Direction
Hexcel® HexWeb® ACG®-1 Honeycomb Aluminum Commercial Grade
HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. ..