Polymer Property : Shear Modulus = 0.00180 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.00180 GPa
0.261 ksi
Typical; ASTM C273
Parabeam Industrie Paraglass 18 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Modulus >= 0.00180 GPa
>= 0.261 ksi
ASTM C273
Parabeam Industrie Paraglass 10 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..