Polymer Property : Shear Modulus = 0.00169 GPa
Polymer Property :
Shear Modulus =
0.00169 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Shear Modulus
0.00169
GPa
0.245
ksi
ASTM D412 Method A
Seals Eastern 7272 Butyl and Halobutyl Rubber
General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc.