Mechanical Properties Metric English Comments
Fracture Toughness 10.0 - 25.0 MPa-m½
9.10 - 22.8 ksi-in½
MMCC Al/B4C Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Fracture Toughness 15.0 - 25.0 MPa-m½
13.7 - 22.8 ksi-in½
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Fracture Toughness 10.0 - 25.0 MPa-m½
9.10 - 22.8 ksi-in½
MMCC Al/SiC Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).