Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 86.0 MPa-m½ | 78.3 ksi-in½ | K(Q) |
Carpenter Pyrowear® 675 Stainless Steel, Tempered 510°C, Transverse Properties Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c.. |