Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 11.67 MPa-m½ | 10.62 ksi-in½ | |
Ceramic Process Systems AlSiC-8, 70 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |