Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 10.0 - 25.0 MPa-m½ | 9.10 - 22.8 ksi-in½ | |
MMCC Al/B4C Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 15.0 - 25.0 MPa-m½ | 13.7 - 22.8 ksi-in½ | |
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 10.0 - 25.0 MPa-m½ | 9.10 - 22.8 ksi-in½ | |
MMCC Al/SiC Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |