Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | >= 82.0 MPa-m½ | >= 74.6 ksi-in½ | |
Latrobe Marvac 250 VIM-VAR ; 10 in. High Strength Maraging Steel MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Fracture Toughness | >= 82.0 MPa-m½ | >= 74.6 ksi-in½ | |
Latrobe Marvac 250 VIM-VAR ; 5 in. High Strength Maraging Steel MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |