Mechanical Properties Metric English Comments
Tensile Modulus 31.0 GPa
4500 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS)
Information provided by PolyOne
Tensile Modulus 31.0 GPa

@Temperature 23.9 °C
4500 ksi

@Temperature 75.0 °F
Dry; ASTM D3039
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Tensile Modulus 31.0 GPa
4500 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Tensile Modulus 31.0 GPa
4500 ksi
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Tensile Modulus 31.0 GPa
4500 ksi
ISO 527-1
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o..
Tensile Modulus 31.0 GPa
4500 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GC-4H PA*-CF40
Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo..
Tensile Modulus 31.0 GPa
4500 ksi
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..