Mechanical Properties Metric English Comments
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly
LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp DF0069E PC
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific)
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP
LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific)
LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P..
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP
LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized.
Tensile Modulus 14.47 GPa
2099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RVL28 PA 66
LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura..