| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 20.66 GPa | 2996 ksi | 1 mm/min; ISO 527 |
| SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
| Tensile Modulus | 20.66 GPa | 2996 ksi | 1 mm/min; ISO 527 |
| SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
| Tensile Modulus | 20.66 GPa | 2996 ksi | 1 mm/min; ISO 527 |
| SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||