Mechanical Properties Metric English Comments
Tensile Modulus 2.19 GPa
318 ksi
ASTM D882
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant
Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d..
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC
LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific)
LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.19 GPa
318 ksi
ASTM D882
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant
Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio..
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12
LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.19 GPa
318 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS
LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP
SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097..
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Tensile Modulus 2.19 GPa
318 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
Tensile Modulus 2.19 GPa
318 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Tensile Modulus 2.19 GPa
318 ksi
Storage
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy