Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.345 - 0.621 GPa | 50.0 - 90.0 ksi | ASTM D638 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Tensile Modulus | 0.483 - 0.621 GPa | 70.0 - 90.0 ksi | |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Tensile Modulus | 0.483 - 0.621 GPa | 70.0 - 90.0 ksi | |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |