Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 2100 Prime Clear OPS, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 2200 Prime Graphic Arts OPS
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 2600 Envelope Window, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 2700 OPS Lamination, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Tensile Modulus | 1.70 - 3.10 GPa | 247 - 450 ksi | ASTM D638 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 3022-57 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 4022-35 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4022-35 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.69 - 3.10 GPa | 390 - 450 ksi | ASTM D638 |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 1200 Utility Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Tensile Modulus | 2.76 - 3.10 GPa | 400 - 450 ksi | ASTM D790 |
Alcoa KAMA 1100 Prime Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Tensile Modulus | 2.69 - 3.10 GPa | 390 - 450 ksi | ASTM D638 |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |