Polymer Property : Tensile Modulus = 218 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.00 - 1.50 GPa

@Temperature 23.0 °C
145 - 218 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.
Tensile Modulus 1.00 - 1.50 GPa
145 - 218 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF)
Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope..
Tensile Modulus 1.00 - 1.50 GPa
145 - 218 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Ultra High ViscosityUses: Batteries; BinderAdditio..