Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.5 - 14.0 GPa | 1810 - 2030 ksi | ISO 527 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Tensile Modulus | 12.5 - 14.0 GPa | 1810 - 2030 ksi | ISO 527 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |