Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.89 GPa | 999 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NI-20GF/15T FR Polyamide 610 (Nylon 610) Information provided by PolyOne |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | ASTM D638 |
PolyOne Nymax™ MF 1204 40 Black 13 Polyamide 66 (Nylon 66) The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc.. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC (Asia Pacific) LNP* LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2200 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2200R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210F PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210R PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa @Temperature 23.0 °C |
999 ksi @Temperature 73.4 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5201R PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5211R PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific) LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant. |
|||
Tensile Modulus | 6.89 GPa | 999 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-30GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |