Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1050TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn.. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1050ZD96 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and .. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1066ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080TU95 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyExcellent ToughnessInformation provided by Technical Polymers |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080ZD94 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Techn.. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080ZD95 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Tensile Modulus | 6.45 GPa | 935 ksi | ASTM D638 |
Ecomass® 1080ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityMetal Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by T.. |