Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.40 GPa | 928 ksi | |
Radici Radilon® S RV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | |
Plastcom SLOVALEN PH 69 GF 30 LS PP, 30% glass fibre, mod. of mech. prop., UV stability FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. UV stable. Increased strength in comparison with u.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min |
Polimeri Europa KOBLEND PCA PD 935 G4 PC+ABS, 20% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 20% glass fibres, high stiffness, very good dimensional stability. Main application fields: structural non a.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | ISO 527-1,-2 |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | |
LATI Latilub 66-20T G/20-V1 PA66, 20% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is .. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp ZFL34XXC PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZFL34XXC is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features incluce: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East) LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66 LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-25 HM PA66-GF25 Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important pro.. |
|||
Tensile Modulus | 6.39 GPa | 928 ksi | Storage |
Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy Product Description: EPO-TEK®H20E-FC is a two-component, electrically conductive, snap curing epoxy for photovoltaic thin film module stringing, semiconductor packaging and PCB circuit assembly.Adv.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PW0042E PA6, 20% Mineral Filled, Injection Molded PW0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Reinforced, Polyamide 6 Injection MoldingInformation provided by Polymer Technology & Services, the North American exclus.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF3 POM 15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry) Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi.. |
|||
Tensile Modulus | 6.40 GPa @Temperature -40.0 °C |
928 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East) Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu.. |
|||
Tensile Modulus | 6.40 GPa | 928 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |