Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.29 GPa | 912 ksi | Clear Casting |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Tensile Modulus | 6.29 GPa | 912 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 6.29 GPa | 912 ksi | Clear Casting |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |