Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.27 GPa | 910 ksi | ASTM D638 |
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet) |
|||
Tensile Modulus | 6.27 GPa | 910 ksi | ASTM D638 |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Tensile Modulus | 6.28 GPa | 910 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 6.28 GPa | 910 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 6.27 GPa | 910 ksi | ASTM D638 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |