Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.621 - 0.758 GPa | 90.0 - 110 ksi | |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Tensile Modulus | 0.621 GPa | 90.0 ksi | ASTM D638 |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Tensile Modulus | 0.621 GPa | 90.0 ksi | ASTM D638 |
Ecomass® 4703ZD84 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica.. |
|||
Tensile Modulus | >= 0.621 GPa | >= 90.0 ksi | 5% strain; ASTM D790 |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |
|||
Tensile Modulus | 0.621 GPa | 90.0 ksi | TM R050-36 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Tensile Modulus | 0.621 GPa | 90.0 ksi | TM R050-36 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |