Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.859 GPa | 849.8 ksi | ISO 527-2/1A/1 |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |