Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.70 GPa | 827 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF43 Nylon 6, 43% Glass Reinforced, Conditioned Nylon 6 - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1,2 |
Qualchem Danamid FGF-15 Polyamide 6, 15% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1,2 |
Qualchem Danamid FGF-20 Polyamide 6, 20% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE15315 BK010 PBT
(Unverified Data**) Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK602 BK851 PBT
(Unverified Data**) Crastin® SK602 BK851 is a 15% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow) |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Durethan® BM 25 FN20 700350 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | |
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Tensile Modulus | 5.70 GPa @Temperature 80.0 °C |
827 ksi @Temperature 176 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161... |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin contaninig Glass Fiber. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East) NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30) 20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free) |
|||
Tensile Modulus | 5.70 GPa @Temperature 160 °C |
827 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK602 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 BK851 is a 15% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1mm/min; ISO 527 |
BASF Ultradur B 4300 G3 BK5110 15% Glass Filled PBT Ultradur B4300 G3 is an easy flowing 15% glass reinforced grade of PBT for injection molding. It is suitable for industrial articles requiring high rigidity, toughness and dimensional stability. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | XY direction; ASTM D638 |
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer Information provided by Advanced Laser Materials (ALM). |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ASTM D638 |
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 80.0 °C |
827 ksi @Temperature 176 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 40YM243 PP SABIC® STAMAX 40YM243 is a 40% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS .. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Durethan® BM 25 FN20 DUS013 000000 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen, optimized for laser marking at 1064 nm, |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PFB42EU PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42EU is a compound based on PA 6 resin containing Glass Fiber, Glass Bead. Added features include Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |