Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.69 GPa | 825 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Tensile Modulus | 5.69 GPa | 825 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Tensile Modulus | 5.69 GPa | 825 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |