Polymer Property : Tensile Modulus = 761 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.25 GPa
761 ksi
Plastcom SLOVAMID 66/6 T 30 TS PA66/6, 30% mineral filling
FeaturesPA 66/PA 6 alloy with the content of 30 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, autom..
Tensile Modulus 5.25 GPa
761 ksi
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Tensile Modulus 5.25 GPa
761 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Tensile Modulus 5.25 GPa
761 ksi
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Tensile Modulus 5.25 GPa
761 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East)
15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors.
Tensile Modulus 5.25 GPa
761 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS
LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Tensile Modulus 5.25 GPa
761 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.