Mechanical Properties Metric English Comments
Tensile Modulus 5.15 GPa
747 ksi
ISO 527
Polyram Polytron P20B11 Polypropylene, 20% Long Fiber Glass
A chemically coupled 20% long fiber glass reinforced black polypropylene, heat stabilized for injection molding applications.Information provided by Polyram.
Tensile Modulus 5.15 GPa
747 ksi
ASTM-D790
Polyram Polytron P20B01 Homopolymer Polypropylene, Chemically Coupled 20% Long Fiber
A CHEMICALLY COUPLED 20% LONG FIBER GLASS REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Tensile Modulus 5.15 GPa
747 ksi
STN EN ISO 527-2
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc