Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.10 GPa | 740 ksi | |
Plastcom SLOVALEN PH 69 GF 20 T 10 PP, 20% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre and 10 % Talc, contains themodifier of mechanical properties.Increased strength in comparison with .. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | |
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 175 °C |
740 ksi @Temperature 347 °F |
Conditioned; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527-1/-2 |
Lanxess Pocan® KU 1-7625 901510 PBT + PC, 20% Glass Fiber PBT+PC, 20% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | |
LATI Latishield 87/28-10A G/20 PC, Steel/Glass Fiber Reinforced EMI shielding product based on Polycarbonate (PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 175 °C |
740 ksi @Temperature 347 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 5.10 GPa @Temperature 175 °C |
740 ksi @Temperature 347 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527-1/-2 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MR 309 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.10 GPa @Temperature 200 °C |
740 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 6027 POM Copolymer, 30% mineral reinforced POM-MD30Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry) Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper Information provided by Asahi Thermofil |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Tensile Modulus | 5.10 GPa | 740 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |