Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0500 GPa | 7.25 ksi | ISO 527-1/-2 |
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | ISO 527-1/-2 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | ISO 527-1/-2 |
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | ISO 527-1/-2 |
DSM Arnitel® EM400-BP TPC-ET 34 Shore D, Injection Molding or Extrusion Grade |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | 1 mm/min |
Arkema Group Evatane® 1003 VL 4S Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for transparent and thermal agricultural film to 180 at 200 µ for greenhouse coverage.ISO data prov.. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | 1 mm/min |
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | 1 mm/min |
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | 1 mm/min |
Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Tensile Modulus | >= 0.0500 GPa | >= 7.25 ksi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | 1 mm/min |
Arkema Group Evatane® 1020 VG 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high mechanical properties. Examples: films, chemical bags, gloves.ISO data provided by the manufactur.. |
|||
Tensile Modulus | 0.0500 GPa | 7.25 ksi | ISO 527-1/-2 |
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | >= 0.0500 GPa | >= 7.25 ksi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |