Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ASTM D638 |
PolyOne Lubri-Tech™ PK-000/15T Polyetheretherketone - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
DSM Akulon® K224-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ASTM D638 |
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ASTM D638 |
Loxim 220 12V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | |
LATI Latilub 62-06GR PA6, Graphite Reinforced Self-lubricating product based on Polyamide 6 (PA6). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, Conditioned Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2212 PEI (Europe-Africa-Middle East) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 1760T PBT+PC (Europe-Africa-Middle East) XENOY 1760T is developed as a easy flow material, for applications such as doorhandles and mirror housings. It is a 11% glass reinforced material with excellent strength and dimensional stability.Th.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX8110P PPE+PA (Europe-Africa-Middle East) GTX8110P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaksThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an.. |
|||
Tensile Modulus | 4.50 GPa @Temperature 100 °C |
653 ksi @Temperature 212 °F |
ISO 527-2 |
Borealis Xmod™ GB305HP High Performance 35% Glass Fiber Reinforced Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1, 2 |
Polyplastics Duracon® TR-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber 15% Glass fiber reinforced polypropylene for injection molding application.Information provided by Polyram. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Tensile Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 5011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527-1/-2 |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 30 HWCP 30% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | |
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced Heat resistant grade with halogen-free flame retardant; applications include TV plug connectors and components in switchgear cabinets.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | |
BASF Procom® T40H 550 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 4.50 GPa | 653 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |