Polymer Property : Tensile Modulus = 55100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 380 GPa
55100 ksi
UBE Tyranno Grade SA Ceramic High Temperature Fiber
Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e..
Tensile Modulus 380 GPa
55100 ksi
Young's; DINV ENV 843-2
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Tensile Modulus 380 GPa
55100 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec 975 Alumina, 99.5%
975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high d..