Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527-1/-2 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | |
Radici Radilon® S RV150 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6 Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 3.75 GPa @Temperature 23.0 °C |
544 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527 |
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527 |
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 3.75 GPa | 544 ksi | ISO 527 |
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |