Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO.527 DIN.53455 |
Omnia Plastica PEEK Polyetheretherketone Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance w.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
Nilit FRIANYL A63 RV0 9005 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East) LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.Thi.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is .. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527; DIN 53452 |
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK) Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metalls semi-crystalline high performance thermoplastic which exhibits a unique combination of high m.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1010N2 1ES NAT PA6 FR(30) Injection Molding, Flame Retardant (Halogen free) |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | DIN 53 457 |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336M40CL Mica Reinforced Coupled |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L1 Wollastonite Reinforced |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339W40L Wollastonite Reinforced |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | |
BASF Procom® GC20S 400 Polypropylene Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer HP0335W40L Wollastonite Reinforced |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | |
Radici Radilon® A HSK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-2 |
CENTROPLAST CENTROLYTE Polyethylene terephthalate This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance. Applications include pump components, coil bodies, ball bearing cups and prote.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |